Fluoropolymer tubing remains resistant at fuming-acid concentrations where PVDF fails, per file's engineering-rules cross-reference.
Materials documented for this service
- FEP/PFA/PTFE/ECTFE (remain resistant)
- PVDF (fails at fuming concentrations)
Products cited for this service
Real Specifications
| ALTAFLUOR 400 PFA temperature ceiling | 500°F upper service temperature | altaflo-fluoropolymer-tubing.md |
| ALTAFLUOR 200 FEP temperature ceiling | 400°F upper service temperature | altaflo-fluoropolymer-tubing.md |
| ALTAFLUOR 480 UHP PFA purity grade | Made exclusively from a high molecular weight, high-purity resin; explicitly rated resistant to common fluorosurfactants | altaflo-fluoropolymer-tubing.md |
| Altaflo 100 PTFE temperature range | -410°F to 500°F continuous service, 550°F short-term — broadest range in the Altaflo line | pexco-tubing.md |
| Altaflo 500 PVDF temperature ceiling | -20°F to 250°F, made from 100% virgin Kynar 740 homopolymer resin | pexco-tubing.md |
Altaflo 100 PTFE and Altaflo 500 PVDF are both explicitly rated not suitable for flare-type fittings — a real fitting-compatibility caveat that matters when specifying tubing hardware for a high-temperature acid transfer line in this family.
Fuming sulfuric acid and oleum push tubing past where PVDF's 250°F ceiling holds up — ALTAFLUOR 400 PFA's 500°F rating and Altaflo 100 PTFE's -410°F to 500°F range are the real ceilings to check before assuming any "fluoropolymer tubing" handles the most aggressive acid concentrations a process can throw at it.
Every material and product claim on this page traces to real, vendor-published documentation on file with LibertyCES. Chemical compatibility depends on exact concentration, temperature, and duty cycle — confirm current specifications with the manufacturer and request a spec review before final specification.
FAQ
Is Tubing compatible with Acids?
Fluoropolymer tubing remains resistant at fuming-acid concentrations where PVDF fails, per file's engineering-rules cross-reference. This is strong evidence.
What materials are documented for Tubing in Acids service?
Materials documented for this service: FEP/PFA/PTFE/ECTFE (remain resistant), PVDF (fails at fuming concentrations). Chemical compatibility depends on exact concentration, temperature, and duty cycle — confirm with a spec review before final specification.
What specific Acids chemicals does this cover?
Named chemicals in this documentation: Sulfuric Acid (98%, fuming/oleum).
What products are cited for Tubing in Acids service?
Documented examples include Altaflo/Pexco ALTAFLUOR 200/350/400/480.